Identification: DIOLEYL HYDROGEN PHOSPHITE CAS: 64051-29-2 Available in: Asia Pacific, Europe, Latin America and North America Applications: DURAPHOS AP-240-L is a thermally stable phenol-free additive used in lube applications for metalworking fluids and in limited slip oil formulations. Its pentavalent structure and high molecular weight help it resist hydrolysis. This dioleyl phosphate assists in applications calling for a “waxy type” additive, similar to the performance previously obtained from sperm whale oil. Information provided by Rhodia, Rhodia has been acquired by Solvay. |