MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Clariant Blue Polycarbonate 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Due to its strength, impact resistance and chemical resistance, polycarbonate is a very attractive material for engineering products. Clariant polycarbonate 3D printer filament is made with a high performance, general purpose and high flow polycarbonate that provides end use parts of excellent quality. A specially formulated Renol® masterbatch is added to improve the processability during 3D printing. Blue color is organic-based.

General properties:

  • Amorphous thermoplastic
  • Strong and tough engineering thermoplastic
  • High impact strength
  • Highly transparent material
Available in a variety of standard colors.

Information provided by Clariant.

Vendors:
Available Properties
  • Density, ISO 1183, (Natural Color)
  • Tensile Strength, Yield, ISO 527, 50 mm/min, Injection Molded
  • Elongation at Break, ISO 527, 50 mm/min, Injection Molded
  • Flexural Strength, ISO 178, Injection Molded
  • Flexural Modulus, ISO 178, Injection Molded
  • Izod Impact, Notched (ISO), ISO 180, Injection Molded
  • Charpy Impact, Notched, ISO 180, Injection Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, Injection Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75, 3D Printed XY / flat at 280°C
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, Injection Molded
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, 3D Printed XY / flat at 280°C
  • Glass Transition Temp, Tg, ISO 11357, DSC at 10°C/min (Natural Color)
  • Processing Temperature, Print Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.