MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Go Yen Chemical Goyenchem-BL430 High Effective Blue Light Blocking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Goyenchem BL-430 can block off high energy short wave blue light 380nm~420nm, and it can be added to the antiblue light goggles, glasses, sunglasses and other kinds of 3C industry. And it also uses to the anti-blue light film, paint, ink, PMMA, PET, PC sheet extrusion, electronic, optical and other applications by well-known manufacturers.

Advantages:

  • High effective UV-absorbent for plastic, fiber and paint
  • Long life UV-barrier effect
  • Effectively block the transmittance of blue light
  • Extend the barrier range to longer wavelength and visible light, and the main wavelength can block off the high energy short wavelength blue light 370nm~440nm. The strongest barrier is about 350nm~410nm.
  • Low volatility
  • Excellent processability
Applications:
  • Goggles, spectacles, sunglasses
  • Paint
  • PET
  • Electron & Optics application
  • Anti-ray film
  • Ink and acrylic resin
  • PC
  • PMMA
  • Screen film
  • Extruded sheet
  • Other application

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Ash
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.