Product description: GENIOSIL® WP 1 is a silane-terminated hybrid polymer. Properties: Formulations with GENIOSIL® WP 1 are characterized by the following advantages: - Simple compounding with conventional auxiliaries.
- Wide variety of formulations thanks to low viscosity, resulting in easily customizable end product properties.
- High mechanical strength and high-modulus formulation feasible.
- Cures quickly, forming a non-tacky surface
- Tin-free catalysis.
- Adheres well to a wide range of surfaces
Low-viscosity end products without the addition of solvents or plasticizersSpecial features: GENIOSIL® WP 1 is a silane-terminated hybrid polymer with very low viscosity. It reacts with moisture to form silanols, which can react further to produce stable siloxane compounds. Application: GENIOSIL® WP 1 is used as a reactive binder for especially low viscous, spreadable, rollable or airless sprayable formulations. Curing takes place in the presence of water or atmospheric moisture. It can be variously formulated to produce compounds of very different viscosities, suitable for waterproofing of vertical as well as horizontal surfaces, including: - Waterproofing of flat roofs, balconies and patios
- Undertile Coatings
- blocking moisture under floor screeds
- Waterproofing of interior and exterior basement walls
- Potting compound for horizontal expansion and movement joints
Information provided by Wacker Chemie AG. |