MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Indium Corp. EZ-Pour® GaCl3 Gallium Trichloride, Anhydrous
Categories: Ceramic; Halide

Material Notes: EZ-Pour® Gallium Trichloride is a granulated, free-flowing form of GaCl3. It is exceptionally easy to handle and can be poured easily from the container. No melting or use of solvents is required.
  • Synonyms: Gallium Chloride, Gallium (III) Chloride
  • CAS Number: 13450-90-3
  • EC Number: 236-610-0
  • RTECS: LW9100000
  • Purity: 99.999% Gallium Trichloride
  • Appearance: White quasi-spherical pellets; Deliquescent; Fumes in Air
  • Form: Free-Flowing Granule
  • Solubility: Soluble in Water, Ammonia, Benzene, Ethers, Carbon Disulfide, Carbon Tetrachloride.

Information Provided by Indium Corporation

Vendors:
Available Properties
  • Density, Solid
  • Density, Liquid at mp
  • Molecular Weight
  • Vapor Pressure
  • Vapor Pressure
  • Melting Point
  • Boiling Point
  • Aluminum, Al, Typical
  • Aluminum, Al
  • Copper, Cu, Typical
  • Copper, Cu
  • Gallium, Ga, Theoretical
  • Germanium, Ge, Typical
  • Germanium, Ge
  • Indium, In, Typical
  • Indium, In
  • Iron, Fe, Typical
  • Iron, Fe
  • Lead, Pb, Typical
  • Lead, Pb
  • Nickel, Ni
  • Sodium, Na, Typical
  • Sodium, Na
  • Tin, Sn, Typical
  • Tin, Sn
  • Trace Metals, Total combined metal impuritiess, typical
  • Trace Metals, Total combined metal impurities
  • Zinc, Zn, Typical
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Indium Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.