MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Teknor Apex Medalist® MD-84368 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-84300 series are high performance thermoplastic elastomer designed specifically for extrusion and injection molded electrical applications in the medical and healthcare industry. The Medalist MD-84300 series are a better alternative to traditional TPVs used in such applications. Medalist MD-84368 is a medium hardness, low density grade with good electrical properties and can be sterilized by autoclave, ETO, or gamma radiation.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Electrically Insulating; Ethylene Oxide Sterilizable; Good Color Stability; Good Colorability; Good Sterilizability; Halogen Free; High Tensile Strength; Low Flow; Low Specific Gravity; Medium Hardness; Radiation Sterilizable; Slip

Uses: Flexible Jacketing; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Wire & Cable Applications

Agency Ratings: ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, ASTM D412
  • Tensile Strength at Break, ASTM D412, in IRM 902 Oil
  • Tensile Strength at Break, ASTM D412, in Air
  • Tensile Stress at Strain, ASTM D412
  • Tensile Stress at Strain, ASTM D412
  • Elongation at Break, ASTM D412
  • Elongation at Break, ASTM D412, in IRM 902 Oil
  • Elongation at Break, ASTM D412, in Air
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Brittleness Temperature, ASTM D746
  • Flammability, UL94, NT
  • Oxygen Index, ASTM D2863
  • Processing Temperature, Melt, Injection
  • Rear Barrel Temperature, Injection
  • Middle Barrel Temperature, Injection
  • Front Barrel Temperature, Injection
  • Nozzle Temperature, Injection
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 4, Extrusion
  • Zone 5, Extrusion
  • Die Temperature, Extrusion
  • Mold Temperature, Injection
  • Injection Pressure, Injection
  • Back Pressure, Injection
  • Cushion, Injection
  • Screw Speed, Extrusion
  • Screw Speed, Injection
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.