MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Copper, UNS C62300 (Aluminum Bronze 9%), H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Good Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Brazing

Common Fabrication Processes: Bending; Forging; Hot forging; Hot Pressing; Welding

Typical uses: Bolts; Nuts; Bearing Races; Bearings; Cams; Gears; Pump Rods; Valve Guides; Valve Seats; Valve Stems; Worm Gears; Marine Hardware

Applicable Specifications: Bar – ASTM B124/B124M, SAE J463, SAE J461, AMS 4635; Die – Forgings AMS 4635, Forgings SAE J463, Forgings SAE J461, Forgings MILITARY MIL-B-16166; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Rod – ASTM B124/B124M, SAE J461, AMS 4635, SAE J463; Rod, Bar & Shapes - Aluminum Bronze ASME SB150, Aluminum Bronze ASTM B150/B150M; Shapes – ASTM B124/B124M

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell B
  • Hardness, Rockwell B
  • Hardness, Rockwell B
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength, Yield, 0.5% Ext
  • Tensile Strength, Yield, 0.5% Ext
  • Tensile Strength, Yield, 0.5% Ext
  • Tensile Strength, Yield, 0.5% Ext
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Tensile Modulus
  • Modulus of Rigidity
  • Poissons Ratio, Calculated
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Fatigue Strength
  • Machinability
  • Forgeability
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Electrical Resistivity, 12% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Hot-Working Temperature
  • Aluminum, Al
  • Copper, Cu, As Balance
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Tin, Sn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.