MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Taiwan PU CPU-107-329A-A Pure Polyurea Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Key features:
  • Hardness: 86-90 shore A
  • Mixing ratio: 1:1 by volume
  • 100% solid content
  • Fast curing
  • High chemical resistance
  • No catalyst content OCs
Description: Pure polyurea coating CPU-107-329A-A/B two component pure polyurea spraying elastomer. It has more outstanding reaction characteristic, physical properties, chemical resistance and abrasion resistance than the general type spraying elastomer.

Application:

  • Highway and bridge overlays
  • Watertight coating
  • Roller, other casting elastomer replacement
  • Protective coating
  • Spray-mold type
  • Abrasion-resistant coating
  • Pipe coating
  • Industrial coating
  • Roof and deck coating
  • Construction coating
Characteristics:
  • Great chemical resistance.
  • Water insensitivity- The curing of CPU-107-329A-A/B is affected very little by dampness, humidity.
  • 100% solid content- Without the aid of solvents or diluents that can evaporate and pollute the environment.
  • Excellent physical properties - Including elongation, tensile strength and abrasion resistance.
  • Consistent reactivity- No catalysts content.
  • Fast reactivity and curing- Generally gel within 3-5 seconds after mixing and cured to walk on within 30 seconds. Can be sprayed on sloped or vertical surface without drips or runs

Information provided by Taiwan PU Corporation

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Tear Strength
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.