MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
HP Alloys HPA COBALT Alloy 6BH, Wear Resistant, (Co-Cr-W) (UNS R30016)
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Cobalt 6BH is the same composition of Cobalt 6B, except the material is hot rolled and then age hardened. The direct age-hardening after hot rolling provides the maximum hardness and wear resistance. The advantages this creates are increased wear life, retained edge characteristics, and increased hardness. These properties are in addition to the galling and seizing resistance of the regular Cobalt 6B.

Cobalt 6BH is known in the industry as a metal that retains its cutting edge. The economic advantages are in its long wear time, less down time, and fewer replacements.

Applications:Steam turbine erosion shields, Chain saw guide bars, High temperature bearings, Furnace fan blades, Valve stems, Food processing equipment, Needle valves, Centrifuge liners, Hot extrusion dies, Forming dies, Nozzles, Extruder screws, & many other Misc. wear surfaces. End uses for alloy 6BH also include tile making machines, rock crushing rollers and cement and steel mill equipment. Alloy 6BH is well suited for valve parts, pump plungers

Wrought alloy 6BH offers the fatigue resistance and toughness of a hot worked microstructure, with the heat corrosion and wear resistance of cobalt based alloy. High Performance Alloys, Inc. inventories sheet, and plate. Bar is can be produced 1/2" through 2-1/2" diameter. Bar can be supplied in random lengths or cut to order. Sheet and plate are offered as whole plates, can be abrasive cut, or processed further using waterjet services.

Data provided by High Performance Alloys, Inc.

Key Words: AMS 5894; High Performance Alloys, Inc.
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Estimated from Rockwell C
  • Hardness, Rockwell A, Estimated from Rockwell C
  • Hardness, Rockwell C
  • Hardness, Vickers, Estimated from Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
High Performance Alloys, Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.