Applications: Specifically designed for foam process, Blends with LLDPE
Additives: Good heat sealing latitude, Moderate toughness, Easy processability
Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions.
Information provided by NOVA Chemicals.