MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
LyondellBasell Petrothene® LP540200 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Applications
PETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-00 is recommended for merchandise bags and multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machinability.

Regulatory Status
LP 5402-00 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of olefin polymer in “...articles or components of articles intended for use in contact with food.” Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing LP 5402-00 can only be made when the processing conditions, equipment and end use are known.
These are typical values and not to be construed as specific product limits.
Data obtained from film produced in a 3½ in. (89 mm) blown film line, commercials available 8'”(203 mm) die, 415°F (213°C) melt extrusion temperature, 2.5:1 BUR, 1.25 mil

This product is from the former Equistar product line.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Water Vapor Transmission, ASTM F372
  • Environmental Stress Crack Resistance, ASTM D1693, Molded; F50
  • Thickness, 2.5:1 BUR
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240, Molded
  • Tensile Strength, Yield, ASTM D638, Molded
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Tensile Impact, ASTM D1822
  • Dart Drop Test, ASTM D1709, F50
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Molded
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746, Molded
  • Melt Temperature
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.