MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Phillips 66 Kendall® Super-D® 3 Diesel Engine Oil-Monograde SAE Grade 50  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Kendall® Super-D 3 monograde diesel engine oils are high-quality diesel engine oils designed for use in a wide variety of applications, including off-highway diesel equipment, farm machinery, marine engines, 2-stroke cycle diesel engines (in the appropriate viscosity grades) and mixed commercial fleets. They also may be used in some heavy-duty manual transmissions in trucks and buses. Super-D 3 monograde diesel engine oils are formulated to provide excellent wear protection, to minimize the formation of sludge and varnish, to protect against rust and bearing corrosion, and to resist foaming. They have excellent soot dispersancy to protect against abrasive wear and soot-induced oil thickening, and excellent oxidation resistance to help minimize deposit formation. The SAE 30 and 40 grades have low ash content to help minimize the formation of ash deposits on valve seats and faces, and help keep intake ports clear to maintain good power output in 2-stroke cycle applications. Super-D 3 SAE 30 and 40 meet or exceed the performance requirements of API Service Categories CF-2 and CF, and also may be used in applications where API CD quality oils are specified. They are particularly recommended for use in 2-stroke cycle diesel engines in transit buses and marine fleets running on low-sulfur diesel fuel. Super-D 3 SAE 50 meets or exceeds the performance requirements of API Service Categories CF and SL. It is primarily recommended for use in off-highway diesel equipment and mixed commercial fleets with both diesel and gasoline vehicles. Super-D 3 SAE 10W is intended for use in the hydraulic systems and hydrostatic transmissions of Caterpillar and other off-highway construction equipment. It is not recommended for use in engines

Applications:

  • 2-stroke cycle diesel engines in bus fleets and marine fleets (SAE 30, 40)
  • Off-highway trucks, heavy equipment and farm equipment
  • Light trucks and farm equipment with gasoline engines (SAE 50)
  • Heavy-duty manual transmissions in trucks and buses where the OEM specifies engine oil (SAE 30, 40, 50)
  • Hydraulic systems and some hydrostatic transmissions on Caterpillar and other off-highway equipment
Super-D 3 monograde diesel engine oils meet or exceed the requirements of:
  • API Service CF-2(1), CF(1) (SAE 30, 40)
  • API Service CF(1), SL (SAE 50)
  • U.S. Military MIL-PRF-2104G, for engines (SAE 30, 40)
  • Detroit Diesel 2-stroke cycle engines, Oil Type 1 (1.0% max. SASH) (SAE 40)
Features/Benefits:
  • Excellent soot control for protection against abrasive wear and soot-induced oil thickening
  • Protects against sludge and varnish formation
  • Protects against scuffing and wear
  • Protects against rust and bearing corrosion
  • Good resistance to foaming and aeration
  • Low-ash content to minimize the formation of ash deposits and help keep intake ports clean (SAE 30 & 40)

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity, High-Temp/High-Shear
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, ASTM D874, Sulfated
  • ASTM Color, ASTM D1500
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point, COC
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.