MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
Categories: Carbon; Diamond; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Metal-doped Me/a-C:H/a-Si:O nanocomposite. The electrical characteristics of these coatings can be tailored by the addition of metal dopants. This creates an engineered surface for specialized applications requiring a combination of wear, low friction, and electrical conductivity. Typical applications include those requiring static discharge in addition to wear resistance, such as in wafer manufacturing.

Applied using a PACVD (plasma-assisted physical vapor deposition) coating method. Diamond-like coatings are amorphous carbon-based coatings that exhibit high hardness and low coefficients of friction. Their unique composition and structure result in excellent wear resistance and non-stick characteristics. These coatings are thin, chemically inert, corrosion resistant, have minimal particulate contamination, tailorable electrical resistivities, and have a very low surface roughness.

Information provided by Bekaert Advanced Coating Technologies (BACT).

Vendors:
Available Properties
  • Thickness, Coating Thickness
  • Hardness, Rockwell C
  • Coefficient of Friction, Dry vs. Steel
  • K (wear) Factor
  • Electrical Resistivity
  • Maximum Service Temperature, Air
  • Processing Temperature, Coating Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Bekaert Advanced Coating Technologies (BACT)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.