MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Solvay ALKAMULS® EL 620 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HLB of around 12. Nonionic emulsifier for metal working formulations. Emulsifier for oils, fatty acids, solvents and waxes in water based formulations. Often used in textile lubricants, and in food contact formulations. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling.

Identification: CASTOR OIL ETHOXYLATE(30)

CAS: 61791-12-6

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Soluble in water

Applications: ALKAMULS EL-620 is a castor oil ethoxylate with a HLB of 12. Emulsifier for oil and waxes in water based formulations. Used as dispersant or pigments and iron powders.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors:
Available Properties
  • Density
  • pH, 7% Solution
  • Viscosity
  • Total Acid Number, RP-0616, [mg KOH/g]
  • Gardner Color Number, RP-0138
  • Shelf Life
  • H2O, Water, RP-0327, Karl Fisher
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.