| Available Properties |
|---|
- Density, ISO 1183, DAM
- Water Absorption, Sim. to ISO 62, DAM
- Moisture Absorption, Sim. to ISO 62, DAM
- Water Vapor Transmission, DIS 15106-1/-2, 23°C/85%r.h.; DAM
- Viscosity Number, ISO 307, 1157, 1628, DAM
- Thickness, DAM
- Hardness, Rockwell R, ISO 2039-2, DAM
- Ball Indentation Hardness, ISO 2039-1, H 358/30; DAM
- Tensile Strength, Yield, ISO 527-1/-2, DAM
- Film Elongation at Break, MD, ISO 527-3, DAM
- Film Elongation at Break, TD, ISO 527-3, DAM
- Film Elongation at Yield, MD, ISO 527-3, DAM
- Film Elongation at Yield, TD, ISO 527-3, DAM
- Elongation at Break, ISO 527-1/-2, Nominal; DAM
- Elongation at Yield, ISO 527-1/-2, DAM
- Tensile Modulus, ISO 527-1/-2, 50% RH
- Tensile Modulus, ISO 527-1/-2, DAM
- Flexural Modulus, ISO 178, DAM
- Poissons Ratio, ISO 527-1/-2, DAM
- Poissons Ratio, ISO 527-1/-2, 50%RH
- Izod Impact, Notched (ISO), ISO 180/1A, DAM
- Izod Impact, Notched (ISO), ISO 180/1A, DAM
- Izod Impact, Unnotched (ISO), ISO 180/1U, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, 50% RH
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact Unnotched, ISO 179/1eU, DAM
- Charpy Impact, Notched, ISO 179/1eA, DAM
- Abrasion, ISO 4649, mm3; DAM
- Film Tensile Strength at Break, MD, ISO 527-3, DAM
- Film Tensile Strength at Break, MD, ISO 527-3, DAM
- Film Tensile Strength at Break, TD, ISO 527-3, DAM
- Film Tensile Strength at Break, TD, ISO 527-3, DAM
- Volume Resistivity, IEC 62631-3-1, 50% RH
- Volume Resistivity, IEC 62631-3-1, DAM
- Surface Resistance, IEC 62631-3-2, 50% RH
- Comparative Tracking Index, IEC 60112, 50% RH
- Comparative Tracking Index, IEC 60112, DAM
- CTE, linear, Parallel to Flow, ISO 11359-1/-2, DAM
- CTE, linear, Transverse to Flow, ISO 11359-1/-2, DAM
- Melting Point, ISO 11357-1/-3, 10°C/min; DAM
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2, DAM
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, DAM
- Flame Spread, ISO 3795 (FMVSS 302)
- Haze, ISO 14782, Film; DAM
- Gloss, ISO 2813, 60° Film; DAM
- Melt Temperature, Extrusion
- Melt Temperature, Extrusion Optimum
- Melt Temperature, Injection Optimum
- Melt Temperature, Injection
- Mold Temperature, Injection Optimum
- Mold Temperature, Injection
- Drying Temperature
- Dry Time, Dehumidified Dryer, Injection
- Dry Time, Dehumidified Dryer, Extrusion
- Moisture Content, Extrusion
- Moisture Content, Injection
- Hold Pressure
|
| | |