HSP8340GNH is non-halogen high gloss PS/PPO resin. HSP8340GNH has excellent creep performance in low and high temperature, low water absorption, high flow and high shape resistance property. HSP8340GNH is mainly used in electron & electric parts, OA appliance, fluid engineering, etc.Information provided by Shanghai Kumho Sunny Plastics co, Ltd |