MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI adhesives
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Polystyrene (PS)

Material Notes: Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiation

Applications: Display, medical devices, Office accessories, Small appliances, Break resistant CD jewel boxes, Toys

Injection Speed: Slow to moderate

All molded samples were an 1/8 inch thick unless noted.

General information about ZYLAR®: ZYLAR® acrylic copolymers are The Clear Alternative to polycarbonate, PETG, impact acrylic and clear ABS for applications that demand clarity and toughness and enhanced processing productivity. ZYLAR is a cost effective alternative in injection molding applications, with over 15 years of proven performance.

ZYLAR has proven performance in a variety of applications, including medical, floor care, appliances, consumer goods, office accessories and supplies, pens and mechanical pencils, commercial paper towel dispensers, point of purchase displays, cosmetics packaging, toys, electronics packaging, housewares, consumer & industrial, and other applications.

ZYLAR® acrylic copolymers provide value through enhanced performance, manufacturing productivity, ease of processing, and potential for capital avoidance through utilization of existing (styrenics) equipment and tooling.

Performance Attributes:

  • Crisp clarity
  • Outstanding practical toughness and ductility
  • Balance of toughness and clarity
  • Easily decorated
  • Can be printed, hot stamped or metalized.
  • Gamma, Eto and E-beam sterilizable
  • Can be bonded to flexible PVC
  • Alcohol and lipid resistance
  • Resistance to most industrial and commercial cleaners
  • Resistance to most household cleaners
  • Resistant to most food additives
  • Residential dishwasher safe - top rack
  • Secondary operations include sonic welding, hotplate welding, ultrasonic bonding and adhesive bonding
  • Over-molding capability
Product Capabilities
  • Antistatic and indoor UV grades available
  • Available in natural and pre-colored
  • Color matching capabilities

Customer Productivity & Processing

  • 5 to 25% density advantage means more parts per pound of resin
  • Faster cycle time
  • Reduced energy and labor costs associated with processing
  • Lower processing temperatures by as much as 150F
  • No drying
  • Styrenic processing
  • Better thermal stability
  • More usable regrind and no black specs
  • Product consistency, color consistency
  • Easily colored at the press
  • Easy flow
  • Able to utilize existing tooling for PC, clear ABS, impact acrylic, PETG, polyesters, propionate (CAP), PVC and other polymers

Information provided by NOVA Chemicals.

This specific grade was discontinued prior to the Styrolution acquision of the Zylar® product line.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, ASTM D955
  • Melt Flow, ASTM D1238
  • Styrene Content, Residual Styrene Monomer Content per Berre Laboratory Analytical Methods 0075
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Yield, 0.2 in/min; ASTM D638
  • Elongation at Break, 0.2 in/min; ASTM D638
  • Modulus of Elasticity, 0.2 in/min; ASTM D638
  • Flexural Strength, 0.05 in/min; ASTM D790
  • Flexural Modulus, 0.05 in/min; ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Flammability, UL94
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.