MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Ohara S-FPM 5 Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: S-FPM5 is a glass material with a ?n / ?T closer to zero than conventional FP-based glass materials and is expected to effectively correct refractive index fluctuations (temperature drift) due to temperature changes. In addition, it has a high partial dispersion ratio ?g, F, which is a characteristic of FP-based glass materials and is effective for correcting secondary chromatic aberration. This glass material can be used, not only for in-vehicle camera lenses, but also for other applications such as projector and interchangeable lenses.

Information provided by Ohara Corporation.

Vendors:
Available Properties
  • Specific Gravity
  • Acid Class, SR
  • Hardness, Knoop
  • Modulus of Elasticity
  • Modulus of Rigidity
  • Poissons Ratio
  • Abrasion, Aa
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Transformation Temperature, Tg, per thermal expansion curve
  • Refractive Index
  • Refractive Index
  • Refractive Index
  • Refractive Index
  • Refractive Index, nt (Hg t line)
  • Refractive Index, ns (Cs s line)
  • Refractive Index, nA' (K A' line)
  • Refractive Index, nr (He r line)
  • Refractive Index, nC (H C line)
  • Refractive Index, nC' (Cd C' line)
  • Refractive Index, nHe-Ne
  • Refractive Index, nD
  • Refractive Index, nd (He D line)
  • Refractive Index, ne (Hg e line)
  • Refractive Index, nf (H F line)
  • Refractive Index, nF' (Cd F' line)
  • Refractive Index, nHe-Cd
  • Refractive Index, ng (Hg g line)
  • Refractive Index, nh (Hg h line)
  • Refractive Index, ni (Hg i line)
  • Abbe Number, ν e
  • Abbe Number, ν d
  • Optical Dispersion, Partial Dispersion, nd-nC
  • Optical Dispersion, Partial Dispersion, nC-nA'
  • Optical Dispersion, Partial Dispersion, nh-ng
  • Optical Dispersion, Partial Dispersion, ne-nC'
  • Optical Dispersion, Partial Dispersion, nF'-ne
  • Optical Dispersion, Partial Dispersion, ng-nF
  • Optical Dispersion, Partial Dispersion, ne-nC
  • Optical Dispersion, Partial Dispersion, nC-nt
  • Optical Dispersion, Partial Dispersion, nC'-nt
  • Optical Dispersion, nF-nC
  • Optical Dispersion, nF'-nC'
  • Optical Dispersion, Partial Dispersion, ni-ng
  • Optical Dispersion, Partial Dispersion, ng-nd
  • Optical Dispersion, Partial Dispersion, ni-nF'
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • Transmission, Visible, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • IR Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  • UV Transmittance, Internal Transmission
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.