MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Osterman & Co OsterleneĀ® PPC08N-SHI High Crystallinity Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Product Description: PPC08N-SHI is a high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics and improved cycle time. PPC08N-SHI has balanced stiffness/toughness, fast molding cycle, high impact resistance, high stiffness, medium flow and nucleated. Applications include; appliances, automotive applications, child safety seals, consumer and industrial applications and rigid packaging.

Availability: North America
Additive: Nucleating Agent
Features: Fast Molding Cycle; Good Processability; High Impact Resistance; High Stiffness; High Toughness; Highly Crystalline; Impact Copolymer; Medium Flow; Nucleated
Uses: Appliances; Automotive Applications; Consumer Applications; Industrial Applications; Packaging; Seals
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors:
Available Properties
  • Density
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ISO 527-2/50, Stress
  • Tensile Strength, Yield, ASTM D638, 2.0 in/min
  • Elongation at Yield, ISO 527-2/50, Strain
  • Elongation at Yield, ASTM D638, 2.0 in/min
  • Tensile Modulus, ISO 527-2/1
  • Flexural Modulus, ISO 178, 0.079 in/min
  • Flexural Modulus, ASTM D790A, 0.051 in/min
  • Flexural Modulus, ASTM D790B, 0.51 in/min
  • Izod Impact, Notched (ISO), ASTM D256A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Gardner Impact, ASTM D5420
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2/Bf, Unannealed
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.