MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Greenheart Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Available in large sizes
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Heavy construction, marine and freshwater construction. Bridges, sleepers, etc.

Key Words: Ocotea Rodiaei; Lumber, Timber
Vendors:
Available Properties
  • Specific Gravity, Green, Central/South American Origin
  • Density, 15% Moisture Content
  • Hardness, Wood Indentation, Side Hardness, Green, Central/South American Origin
  • Hardness, Wood Indentation, Side Hardness, 12% Moisture, Central/South American Origin
  • Modulus of Rupture, Static Bending, Green, Central/South American Origin
  • Modulus of Rupture, Static Bending, 12% Moisture, Central/South American Origin
  • Flexural Modulus, Static Bending, Green, Central/South American Origin
  • Flexural Modulus, Static Bending, 12% Moisture, Central/South American Origin
  • Compressive Strength, Parallel to Grain, Green, Central/South American Origin
  • Compressive Strength, Parallel to Grain, 12% Moisture, Central/South American Origin
  • Machinability, Difficult Relative to Other Wood
  • Shear Strength, Parallel to Grain, Green, Central/South American Origin
  • Shear Strength, Parallel to Grain, 12% Moisture, Central/South American Origin
  • Work to Maximum Load, Static Bending, Green, Central/South American Origin
  • Work to Maximum Load, Static Bending, 12% Moisture, Central/South American Origin
  • Shrinkage, Radial Shrinkage Green to Oven Dry, Central/South American Origin
  • Shrinkage, Tangential Shrinkage Green to Oven Dry, Central/South American Origin
  • Shrinkage, Volumetric Shrinkage Green to Oven Dry, Central/South American Origin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.