MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV159 sealant also provides high temperature performance. It releases acetic acid vapors as a by-products of cure.

RTV159 sealant is a paste consistency product which can be applied to horizontal, vertical, and overhead surfaces in applications requiring high strength and temperature performance.

Since this adhesive sealants utilizes a moisture cure system, it must not be used in thicknesses greater than 6mm(1/4in.). Where section depths exceed 6mm (1/4 in.), GE Silicones one-component, addition cure or two-component silicone rubber compounds are suggested.

This sealant was not designed for and should not be used for applications intended for permanent implantation into the human body.

Mechanical properties for specimen cured 3 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • High strength
  • High temperature performance
  • Low temperature flexibility
  • One-component
  • Room temperature cure
  • General primerless adhesion
  • Excellent electrical insulation properties
  • Excellent weatherability, ozone, and chemical resistance

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors:
Available Properties
  • Specific Gravity
  • Linear Mold Shrinkage
  • Hardness, Shore A
  • Tensile Strength, Ultimate, Cured 7 days at 25°C and 50% relative humidity
  • Elongation at Break
  • Tear Strength
  • Peel Strength, Cured 7 days at 25°C and 50% relative humidity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Brittleness Temperature
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.