MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Attane™ 4704G LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description:
    Provides improved cling in one-sided cling applications
  • It has improved toughness and optical properties
Complies with: US FDA FCN 424; EU No 10/2011. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA FCN 424; EU No 10/2011

Form: Pellets

Processing Method: Cast Film

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882, 100% in cling layer
  • Film Tensile Strength at Yield, MD, ASTM D882, 50% in cling layer
  • Film Tensile Strength at Yield, TD, ASTM D882, 100% in cling layer
  • Film Tensile Strength at Yield, TD, ASTM D882, 50% in cling layer
  • Film Elongation at Break, MD, ASTM D882, 100% in cling layer
  • Film Elongation at Break, MD, ASTM D882, 50% in cling layer
  • Film Elongation at Break, TD, ASTM D882, 50% in cling layer
  • Film Elongation at Break, TD, ASTM D882, 100% in cling layer
  • 1% Secant Modulus, ASTM D882, MD, 100% in cling layer
  • 1% Secant Modulus, ASTM D882, TD, 50% in cling layer
  • 1% Secant Modulus, ASTM D882, TD, 100% in cling layer
  • 1% Secant Modulus, ASTM D882, MD, 50% in cling layer
  • Elmendorf Tear Strength MD, ASTM D1922, 50% in cling layer
  • Elmendorf Tear Strength MD, ASTM D1922, 100% in cling layer
  • Elmendorf Tear Strength TD, ASTM D1922, 100% in cling layer
  • Elmendorf Tear Strength TD, ASTM D1922, 50% in cling layer
  • Film Tensile Strength at Break, MD, ASTM D882, 50% in cling layer
  • Film Tensile Strength at Break, MD, ASTM D882, 100% in cling layer
  • Film Tensile Strength at Break, TD, ASTM D882, 50% in cling layer
  • Film Tensile Strength at Break, TD, ASTM D882, 100% in cling layer
  • Melting Point
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003, 100% in cling layer
  • Haze, ASTM D1003, 50% in cling layer
  • Gloss, ASTM D2457, 45°, 50% in cling layer
  • Gloss, ASTM D2457, 45°, 100% in cling layer
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.