MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL SUPER calcium silicate slabs have the following characteristics:
  • Max. service temperature: Up to 1100°C (2012°F)
  • Back-up insulation only
  • Extremely lightweight
  • Very low thermal conductivity
  • Excellent mechanical strength
  • Can be used in furnaces with reducing atmosphere due to their high resistance to carbon monoxide and hydrocarbons
  • Designed for the application as back-up insulation of all refractory constructions
  • The ideal choice for efficient insulation of kilns, furnaces, ovens, stoves, boilers, soaking pits, regenerators, mains and other combustion equipment
  • The combination of low weight, high service temperature and good integrity makes the calcium silicate slabs highly applicable as fire protection in several applications.

Information provided by Skamol.

Vendors:
Available Properties
  • Bulk Density, Dry
  • Loss On Ignition
  • Porosity, Total
  • Permeability, BS EN 993-4: 1995, nPm, Permeability to Air
  • Modulus of Rupture, EN 993-6: 1995
  • Compressive Strength, EN 1094-5: 1995
  • CTE, linear, BS 1902: section 5.3: 1990
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM C-182, Mean temp.
  • Thermal Conductivity, ASTM C-182
  • Thermal Conductivity, ASTM C-182
  • Maximum Service Temperature, Air
  • Shrinkage, EN 1094-6: 1999, Linear Reheat Shrinkage, 12h at 50°C (122°F) below max. service temp.
  • Al2O3
  • CaO
  • Fe2O3
  • K2O
  • MgO
  • Na2O
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.