Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA. Information provided by Braskem |