MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Kraton® G2705 GU (SEBS) Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good puncture resealing characteristics. It is also steam sterilizable. It is supplied from North America in the physical form identified:
G2705 GU-N - supplied as a transparent pellet.

Region: Asia Pacific, Europe, Japan, North America, and South America

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors:
Available Properties
  • Specific Gravity, BAM 1014
  • Hardness, Shore A, BAM 1003, Injection molded plaque at 205°C
  • Tensile Strength, ASTM D412, Injection molded plaques, Die C, Machine Direction
  • Tensile Strength, ASTM D412, Injection molded plaques, Die C, Cross Direction
  • Elongation at Break, ASTM D412, Injection molded plaques, Die C, Machine Direction
  • Elongation at Yield, ASTM D412, Injection molded plaques, Die C, Cross Direction
  • 100% Modulus, ASTM D412, Injection molded plaques, Die C, Cross Direction
  • 100% Modulus, ASTM D412, Injection molded plaques, Die C, Machine Direction
  • 300% Modulus, ASTM D412, Injection molded plaques, Die C, Cross Direction
  • 300% Modulus, ASTM D412, Injection molded plaques, Die C, Machine Direction
  • Tear Strength, ASTM D624, Injection molded plaques, Die C, Machine Direction
  • Tear Strength, ASTM D624, Injection molded plaques, Die C, Cross Direction
  • Compression Set, ASTM D395B, Injection molded plaque
  • Transmission, Visible, transparent; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.