MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Lord Adhesives CoolTherm™ MD-140 SP Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD CoolTherm™ MD-140 SP silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, power semiconductor and VLSI assembly. CoolTherm MD-140 SP adhesive is low stress, making it suitable for use with large die. CoolTherm MD-140 SP adhesive provides excellent adhesion to a wide variety of surfaces including silicon, silver, gold and copper. Low ionic levels make it ideally suited for demanding semiconductor and hybrid assembly applications.

Features: provides a working life of up to 72 hours after loading a syringe into the dispensing equipment at room temperature. allows high-speed, accurate syringe dispensing of fine dots or lines; can be used with time/pressure, positive displacement or linear dispense heads. rapidly cures at 150°C and 180°C.

All information provided by Lord.

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity
  • Ionic Impurities - Na (Sodium), cured
  • Ionic Impurities - K (Potassium), cured
  • Ionic Impurities - Cl (Chloride), cured
  • Shear Strength, Die Shear, cured
  • Volume Resistivity, cured
  • CTE, linear, alpha 1 cured
  • CTE, linear, alpha 2, cured
  • Thermal Conductivity, cured
  • Glass Transition Temp, Tg, by TMA, cured
  • Cure Time, measured by laser flash method
  • Shelf Life, from date of manufacture when stored in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.