Homopolymer Applications: Staple Fiber and General Purpose Injection Molding Formolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general purpose injection molding applications. It contains a unique combination of stabilizers which give it process stability and end use performance. Specimens were injection molded according to the conditions specified in ASTM D4101. Information provided by Formosa Plastics Corporation, USA. |