MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Henkel Loctite® ECCOBOND EO1016 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Cure: Heat Cure

Product Benefits:

  • Excellent shelf stability
  • Fast curing
  • flame-out
Application: Encapsulant

Typical Application: IC's, transistors and similar semiconductors

LOCTITE ECCOBOND EO1016 is an epoxy encapsulant intended for applications requiring excellent handling properties. The cured material survives severe thermal shock and offers continuous service to 177 °C. It is particularly suited for use on transistors and similar semiconductors, can be used for encapsulation of watch ICs.

Information provided by Loctite®

Vendors:
Available Properties
  • Specific Gravity
  • Moisture Absorption, 24 hours immersion
  • Moisture Absorption, 24 hours immersion
  • Brookfield Viscosity, Spindle 6, speed 20 rpm
  • Brookfield Viscosity, Spindle 6, speed 2 rpm
  • Hardness, Shore D, Cured
  • Tensile Strength, Cured
  • Elongation at Break, Cured
  • Flexural Strength, Cured
  • Flexural Modulus, Cured
  • Adhesive Bond Strength, Cohesive, Al-Al Tensile shear
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dissipation Factor, IEC 60250
  • Arc Resistance, ASTM D495
  • CTE, linear, Cured, Below Tg
  • CTE, linear, Cured, Above Tg
  • Thermal Conductivity, Cured
  • Maximum Service Temperature, Air, DSC, Initial
  • Maximum Service Temperature, Air, DSC, Peak
  • Glass Transition Temp, Tg, Cured
  • Flammability, UL94
  • Shrinkage, 10 grams
  • Cure Time
  • Cure Time, Alternate Cure Schedule
  • Pot Life
  • Gel Time
  • Shelf Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.