MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Teknor Apex SarlinkĀ® TPV X18035 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X18035 is a high performance thermoplastic vulcanizate used in automotive and industrial applications. This product is a low hardness, low density grade exhibiting superior compression set and chemical resistance. This grade can be processed by injection molding and extrusion.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; General Purpose; Good Adhesion; Good Flexibility; Good Moldability; High Elasticity; Low Density; Low Hardness; Resilient

Uses: Automotive Applications; Automotive Interior Parts; Automotive Under the Hood: Diaphragms; Gaskets; General Purpose; Industrial Applications; O-rings; Plugs; Profiles; Rubber Replacement; Seals; Weatherstirpping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, ASTM D3835, Apparent
  • Hardness, Shore A, ISO 868, Extruded
  • Hardness, Shore A, ISO 868, Injection Molded
  • Tensile Strength at Break, ISO 37, Flow
  • Tensile Strength at Break, ISO 37, Across Flow
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Strength at Break, ISO 188, Across Flow, Change in Air
  • Tensile Stress at Strain, ISO 37, Across Flow
  • Tensile Stress at Strain, ISO 37, Flow
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 1008 hr
  • Tensile Stress at Strain, ISO 188, Across Flow, Change in Air at 168 hr
  • Elongation at Break, ISO 37, Flow
  • Elongation at Break, ISO 37, Across Flow
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Elongation at Break, ISO 188, Across Flow, Change in Air
  • Tear Strength, ISO 34-1, Method Ba, Angle (Unnicked), Across Flow
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Processing Temperature, Melt, Injection
  • Rear Barrel Temperature, Injection
  • Middle Barrel Temperature, Injection
  • Front Barrel Temperature, Injection
  • Nozzle Temperature, Injection
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 4, Extrusion
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  • Mold Temperature, Injection
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Teknor Apex Company

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.