MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Mi-Tech Metals Diemitechâ„¢ Tungsten-Based Metal
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available materials, giving it superior refractory properties resulting in greater resistance to erosion and wear. Diemitech maintains good thermal conductivity and physical properties at high working temperatures.

Advantages of using Diemitech:Tools run much cooler because its thermal conductivity is 3-4 times that of steel.
Low thermal expansion - 1/3 that of steel.
Withstands thermal shock.
Excellent mechanical properties at elevated temperatures.
Resists erosion and scaling.
Minimizes soldering and heat checking.
No costly treatment required, normally can be placed into service as machines.
Superior physical properties compared to steel at high working temperatures.
Diemitech is machinable, similar to cast iron.

Data provided by Mi-Tech Metals.

Key Words: Tungsten Alloys
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Ni, Fe, Mo
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.