  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Synthos HI 552M HIPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: High-impact type for a wide range of applications; Processed mainly by injection. Manufacture of consumer goods and technical components which are exposed to higher mechanical stress. Good results are also achieved in the extrusion of profiles.

SYNTHOS PS HI 552M is high-impact polystyrene (HIPS) with a balanced combination of rheological, mechanical and thermal properties, suitable for general application use. It is a thermoplastic material designed for injection moulding and extrusion. SYNTHOS PS HI 552M is a opaque plastic. Product has a form of lens granules of diameter 2,5 to 4 mms. Product may contain small amounts of granulate finer than that mentioned above of irregular shapes. Presence of any mechanical impurities in the granulate is not allowed.

Information provided by Synthos

Vendors:
Available Properties
  • Density, apparent
  • Density, ISO 1183
  • Water Absorption, ISO 62, Ø 50x3 mm
  • Linear Mold Shrinkage, 50x50 mm
  • Melt Flow, ISO 1133
  • Styrene Content, Residual
  • Ball Indentation Hardness, ISO 2039-1, H 358/30, Ø 50x4 mm
  • Tensile Strength at Break, ISO 527-2/1A/5, 5 mm/min
  • Tensile Strength, Yield, ISO 527-2/1A/50, 50 mm/min
  • Elongation at Break, ISO 527-2/1A/5, 5 mm/min
  • Modulus of Elasticity, ISO 527-2/1A/1, 1 mm/min
  • Flexural Strength, ISO 178, 2 mm/min; 80x10x4 mm
  • Izod Impact, Notched (ISO), ISO 180/1A, 80x10x4 mm, r=0,25; V-karb, V-vrub
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80x10x4 mm
  • Charpy Impact Unnotched, ISO 179/1eU, 80x10x4 mm
  • Charpy Impact Unnotched, ISO 179/1fU, 80x10x4 mm
  • Charpy Impact, Notched, ISO 179/1eA, 80x10x4 mm, r=0,25; V-karb, V-vrub
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/Af, 80x10x4 mm
  • Vicat Softening Point, ISO 306/B50, 50 °C/h, 10x10x4 mm
  • Vicat Softening Point, ISO 306/A50, 50 °C/h, 10x10x4 mm
  • Flammability, UL94
  • Melt Temperature, Injection moulding
  • Melt Temperature, Extrusion
  • Mold Temperature, Injection moulding
  • Dry Time, drier with a molecular sieve
  • Dry Time, hot-air drier
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.