MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Global EPP PET SL PET + Solid Lubricant
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechanical precision components subjected to sustained abrasive environments are particularly suited to this material.

Key characteristics:

  • Excellent dimensional stability
  • High mechanical strength, hardness and rigidity
  • Excellent wear resistance
  • Good creep resistance
  • Low moisture absorption
  • Low thermal expansion
  • Good resistance to radiant energy
  • Good electrical insulating properties
  • Stain resistant
  • Suitable for food contact

This internally lubricated grade incorporates a uniformly dispersed solid lubricant; demonstrating improved frictional properties, outstanding wear resistance and excellent pressure-velocity characteristics over the basic grade.

Vendors:
Available Properties
  • Density, ISO 1183:1987, Test Method A
  • Water Absorption, ISO 62:1999 (modified), Immersion
  • Moisture Absorption at Equilibrium, ISO 62:1999, 50% RH
  • Water Absorption at Saturation, ISO 62:1999
  • Tensile Strength at Break, ISO 527-1/2:1993, Sample Type 1B, 50mm/min
  • Elongation at Break, ISO 527-1/2:1993, Sample Type 1B, 50 mm/min
  • Modulus of Elasticity, ISO 527-1/2:1993, Sample Type 1B, 50 mm/min
  • Flexural Strength, ISO 178:2001, 1.5 mm/min
  • Flexural Modulus, ISO 178:2001, 1.5 mm/min
  • Compressive Strength, ISO 604:2002, Sample Type B, 5 mm/min
  • Compressive Modulus, ISO 604:2002, Sample Type A, 1 mm/min
  • Izod Impact, Notched (ISO), ISO 180:2000, Sample Type A
  • Charpy Impact, Notched, ISO 179-2:1999
  • Coefficient of Friction, Dynamic, 31.4 m/min
  • Limiting Pressure Velocity
  • Volume Resistivity, IEC 60093:1980-01
  • Surface Resistance, IEC 60093:1980-01
  • Dielectric Constant, IEC 60250:1969-01
  • Dielectric Constant, IEC 60250:1969-01
  • Dielectric Strength, IEC 60243-1:1998-01
  • Dissipation Factor, IEC 60250:1969-01
  • Comparative Tracking Index, IEC 60112:2003-01
  • CTE, linear, ISO 11359-2:1999
  • Thermal Conductivity, ISO 8301:1991
  • Melting Point
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Minimum Service Temperature, Air, Continuous
  • Glass Transition Temp, Tg, ISO 11359-2:1999
  • Flammability, UL94, IEC 60695-11-10:2003-08
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.