MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an inherent static dissipative polymer network. This inherent static dissipative network remains intact through injection molding or extruding while maintaining the physical properties of TPU. Stat-Rite® TPU alloys are formulated for permanent and consistent ESD protection without comprising cleanliness.

Features:

  • Permanently static dissipative
  • Does not require humidity
  • Ultra-Clean: low off-gassing, low ionics, low particulates
  • See-through clarity
  • No particulates

Applications:

  • Cleanroom soft walls, windows and doors
  • Electronic component handling
  • Vacuum Tubing
  • Work surface mats

Properties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material two to three hours at 105°C (220°F) in a dehumidifying hopper dryer.

Data provided by Noveon, Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, Yield, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • 300% Modulus, ASTM D412
  • Surface Resistivity per Square, ASTM D257
  • Static Decay, 50% R.H. Charge Plate Monitor
  • Transmission, Visible, Mfr. Specifies transparent but doesn't quantify
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lubrizol (former Noveon)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.