MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Syensqo (Solvay Specialty Polymers) Algoflon® XPH 2530 1N PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® XPH 2530_1N is a white aqueous PTFE dispersion and is produced without any intentional use or addition of PFOA. It is designed for impregnation processes and is particularly recommended for production of fabrics and laminates.
Algoflon® XPH 2530_1N exhibits excellent wetting properties, high shear stability and low foaming formation.

Main features of Algoflon® XPH 2530_1N PTFE dispersion are:
-NO polyethoxylated alkylphenols
-Superior film building behavior
- Excellent surface finishing and gloss
-Very high shear stability

Applications: Coating Applications; Impregnation Applications

Features: Chemical Resistant; High Heat Resistance; Low Friction

Processing
- Algoflon XPH 2530_1N is processed according to methods generally used for conventional impregnation technology. Generally the procedure involves dip-coating and then heating to remove water and surfactant from the impregnated item. Depending on the application, sintering above the crystalline melting point of the coated resin may be carried out to obtain the finished coated articles. Multiple passes may be required to obtain the desired PTFE load and coating thickness.
- Algoflon XPH 2530_1N can be processed neat or appropriately formulated. Also, it can be used diluted using distilled or deionized water. Formulation, line speed and oven temperature must all be well controlled for optimized features of the coated substrates.

Storage and Handling
- Algoflon® PTFE dispersions must be stored under suitable temperature conditions to ensure prolonged stability. Prolonged exposure to temperatures lower than 5°C must be avoided to prevent irreversible settling. Also, some settling may occur on prolonged standing and/or heat exposure. Therefore, it is strongly recommended to keep the product below 35°C.The optimum storage temperature range is 5-25 °C. If the product remains continuously out of the range 5–35 °C for long times, Solvay suggests bringing it in the range 5-25 °C followed by there-homogenization under gentle stirring and the removal of eventual agglomerated particles with a filter of 200 µm and 20 um before the use.
- It is also advisable that the product is homogenized by gentle rolling or stirring once per month and prior to use. Solvay recommends both stirring and filtration for the removal of eventual agglomerate if the product remains in stock for more than three months without gentle stirring.
- Prolonged exposure of the PTFE latex to air could lead to some coagulation at the surface due to water evaporation. For this reason and also to avoid contamination, it is recommended to keep the containers closed when not in use.
- The pH of product must be kept in the range 9.5-11.0 for avoiding bacterial growth that causes odor and scum.
- During handling, violent agitation and pumping must be avoid to minimize agglomeration and foaming formation. It is recommended to convey the dispersion by gravity from its container to the processing station.

Safety and Toxicology
- Before using Algoflon® XPH 2530 1N dispersions consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Venting units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density
  • Particle Size, Average
  • pH, ASTM D4441
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.