MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Deranox™ 995 Alumina Ceramic Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Alumina ceramic of 99.5% Al2O3 content. This material is extensively used for applications that require exceptional electrical resistance combined with resistance to chemical attack.

Prime Features:

  • Ultra-low outgassing
  • Low neutron absorption
  • Resistant to fluorine and chlorine attack
  • Very high volume resistivity
  • Good thermal conductivity
  • Non-porous and vacuum tight
Typical Applications:
  • Gas, solid-state and waveguide lasers
  • Components for a wide range of industrial, medical and defence equipment.
Production Capabilities:
  • Isostatic pressing of components up to 1100mm long
  • Volume production to close dimensional tolerances
  • Surface polishing
  • Glass or thermal diffusion bonding for high quality hermetic sealing
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: Alumina Ceramic
Vendors:
Available Properties
  • Density, fired
  • Open Porosity, fully dense, % nominal, apparent
  • Grain Size
  • Hardness, Rockwell HR45N
  • Hardness, Vickers, [GPa]
  • Modulus of Elasticity
  • Flexural Strength, ASTM C1161, 3-point
  • Compressive Strength
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, ASTM D257
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor, ASTM D2520, tan d
  • Dissipation Factor, ASTM D150, tan d
  • Dissipation Factor, ASTM D2520, tan d
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM E228
  • Thermal Conductivity, ASTM E228
  • Thermal Conductivity, ASTM E228
  • Thermal Conductivity, ASTM E228
  • Thermal Conductivity, ASTM E228
  • Maximum Service Temperature, Air, no load
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.