MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
ChevronTexaco ATF+3® Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: General Description

DaimlerChrysler has had their own ATF specifications for many years, but as of 1997, Chrysler owners manuals no longer list DEXRON as an acceptable replacement. ATF+3 is a readily available mineral oil-based ATF that is suitable in any application calling for ATF PLUS® , ATF+2® , or a Type 7176® fluid. Vehicles manufactured after 1999 require ATF+4® , a synthetic-based ATF only available through DaimlerChrysler.

Chevron ATF+3 is specially formulated to optimize performance of Chrysler transmissions and transaxles.

Applications

Chevron ATF+3 Automatic Transmission Fluid is designed for use in all Chrysler automatic transmissions and automatic transaxles where a Mopar ATF PLUS, ATF+2 or ATF+3 fluid is specified.

It is not recommended for use in transmissions specifying either DEXRON® or MERCON® type fluids

Chevron ATF+3 Automatic Transmission Fluid has been registered with the Chrysler Corporation.

Key Words: CPS Number: 238200; MSDS Number: 6801
Vendors:
Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.