MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Chemours Krytox® XTH-1000 Extreme High Temperature PFPE Oil  (discontinued **)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: These oils are a special extreme high temperature grade with low oil evaporation and have had extra treatment to allow use at temperatures above the range of normal PFPE oils. It has excellent lubrication over a broad temperature range. Krytox® XHT series oils are nonflammable and chemically inert. Krytox® allows extended lubrication intervals and longer equipment life. The oil can begin to slowly degrade at temperatures above 330°C (625°F), and this will occur at an increasing rate as temperatures increase. Relubrication could be required at these temperatures to achieve optimum life. Krytox® PFPE oils are clear, colorless, fluorinated synthetic oils that are nonreactive, nonflammable, safe in chemical and oxygen service, and are long lasting. Krytox® is a perfluoropolyether (PFPE)— also called perfluoroalkylether (PFAE) or perfluoropolyalkylether PFPAE). The polymer chain is completely saturated and contains only carbon, oxygen, and fluorine. On a weight basis, a typical Krytox® oil contains 21.6% carbon, 9.4% oxygen, and 69.0% fluorine.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015. This specific product was discontinued prior to the formation of Chemours.

Vendors:
Available Properties
  • Density
  • Density
  • Viscosity Measurement, Base Oil Viscosity Index
  • Kinematic Viscosity
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Vapor Pressure Test, Knudsen, 20°C
  • Vapor Pressure Test, Knudsen, 100°C
  • Vapor Pressure Test, Knudsen, 200°C
  • Evaporation Loss, Oil Volatility; 22 hr; 260°C
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point, Base Oil
  • Carbon, C
  • Fluorine, F
  • Oxygen, O
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont Performance Lubricants

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.