MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Designer Molecules PEAM-645 Polyester acrylate/methacrylate
Categories: Polymer; Adhesive

Material Notes: Description: PEAM-645 is a polyester acrylate/methacrylate that exhibits low CTE, high Tg, and high modulus. The oligomer has very high thermal stability and low volatility. It can be used as a base resin in a formulation or as an additive. It exhibits good adhesion on various substrates. The oligomer also exhibits good hydrolytic stability.

Highlights:

  • High Tg
  • High adhesion to various substrates
  • Low CTE
  • Thermal stability

Information provided by Designers Molecules

Vendors:
Available Properties
  • Viscosity, Haake Rheometer
  • Molecular Weight
  • Storage Temperature
  • Tensile Modulus, cured with 2% Dicumyl Peroxide
  • Tensile Modulus, cured with 2% Dicumyl Peroxide
  • Tensile Modulus, cured with 2% Dicumyl Peroxide
  • CTE, linear, oc 1, cured with 2% Dicumyl Peroxide
  • CTE, linear, co 2, cured with 2% Dicumyl Peroxide
  • Glass Transition Temp, Tg, TMA, cured with 2% Dicumyl Peroxide
  • Glass Transition Temp, Tg, DMA, cured with 2% Dicumyl Peroxide
  • Decomposition Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.