MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrates and the ability to withstand rigorous thermal cycling. This one component, no mix system is formulated to cure at elevated temperatures e.g. 45-60 minutes at 250-300°F depending on the temperature. The tensile shear strength exceeds 2,700 psi. It is serviceable at cryogenic temperatures from 4K to +400°F. It is 100% reactive and does not contain any diluents or solvents. It has excellent adhesion to most metals, ceramics, glass and vulcanized rubbers, as well as many plastics. Supreme 10AOHT-LO produces durable, high strength, thermally conductive, very tough bonds which are resistant to many chemicals including water, oil, fuels and many acids and bases. One particularly noteworthy feature of this system is its toughness, which imparts resistance to thermal cycling as well as thermal and mechanical shock. It also gives it higher peel strength. It is gray in color. Master Bond Supreme 10AOHT-LO is widely used in electronic, electro-optic, aerospace and specialty applications where high strength, the convenience of a no mix system, excellent thermal transfer properties and high temperature resistance are required. Most importantly, Supreme 10AOHT-LO passes NASA low outgassing testing as per ASTM E595.

Key Features

  • Meets NASA low outgassing specifications
  • Cryogenically serviceable down to 4K
  • Outstanding thermal cycling resistance
  • Great shear and peel strength
  • Withstands temperatures up to 400°F
Product Advantages:
  • Single component system; no mixing prior to use
  • Easy application; contact pressure only required during simple heat cure; spreads evenly & smoothly
  • High peel and shear strengths to a wide variety of substrates
  • Good chemical resistance
  • Great physical strength properties
  • Excellent electrical insulating properties and high thermal conductivity
  • Excellent durability and dimensional stability

Information provided by MasterBond®

Vendors:
Available Properties
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Compressive Strength
  • Shear Strength, Tensile lap, Al to Al
  • Peel Strength, T-peel, Al to Al
  • Volume Resistivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.