MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
EOS 3D Printed StainlessSteel 316L Processed by DMSL on EOSINTM280
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: The parts built from EOS 3D Printed StainlessSteel 316L have chemical composition corresponding to ASTM F138 “Standard Specification for Wrought 18Cr-14Ni-2.5Mo 3D Printed Stainless Steel Bar and Wire for Surgical Implants (UNS S31673)”. This kind of 3D Printed Stainless steel is characterized having a good corrosion resistance and evidence that there are no leachable substances in cytotoxic concentrations. This material is ideal in
  • Lifestyle/Consumer - watches, other jewelry, spectacle frames, decorations, functional elements in electronic housing and accessories
  • Automotive/Industrial – non-corroding common material, food and chemical plants
  • Aerospace/Turbine industry – entry-level material for Laser Sintering Technology, mounting parts, brackets, heat exchangers
Parts built from EOS 3D Printed StainlessSteel 316L can be machined, shot-peened and polished in as-built or stress relieved (AMS2759) states if required. Solution annealing is not necessary because the mechanical properties of as-built state are showing desired values (ASTM A403). Parts are not ideal in temperature range 427°C - 816°C where precipitation of chromium carbides occurs. Due to layer-wise building method, the parts have a certain anisotropy which could be seen from mechanical properties.

Information provided by Proto3000

Key Words: Direct Metal Laser Sintering
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, EN ISO6508-1
  • Tensile Strength, Ultimate, ISO 6892 / ASTM E8M, in vertical direction (Z)
  • Tensile Strength, Ultimate, ISO 6892 / ASTM E8M, in horizontal direction (XY)
  • Tensile Strength, Yield, ISO 6892 / ASTM E8M, in vertical direction (Z)
  • Tensile Strength, Yield, ISO 6892 / ASTM E8M, in horizontal direction (XY)
  • Elongation at Break, ISO 6892 / ASTM E8M, in horizontal direction (XY)
  • Elongation at Break, ISO 6892 / ASTM E8M, in vertical direction (Z)
  • Modulus of Elasticity, ISO 6892 / ASTM E8M, in vertical direction (Z)
  • Modulus of Elasticity, ISO 6892 / ASTM E8M, in horizontal direction (XY)
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe, Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Nitrogen, N
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Electro Optical Systems GMBH

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.