MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric acid solutions. The silicon content is kept under 0.3% while the carbon content is lower than 0.015%. Molybdenum additions are also well known to reduce the behavior of the steel in nitric acid solutions. This explains why the molybdenum content is guaranteed lower than 0.3%. The sharp control of Carbon, Silicon and phosphorus contents makes it possible to produce a more stable austenite microstructure, free of intermetallic or carbide precipitations. The alloy is designed for nitric acid applications. The grade is not recommended for concentrated nitric acid purposes or highly oxidizing nitric acid solutions (with Gr VI species...)

Information provided by manufacturer.

Key Words: EURONORM X1 Cr Ni 25.21 - 1.4335, AFNOR Z1 CN 25.20, WERKSTOFF Nr 1.4335, ASTM 310 L NAG
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Average
  • Tensile Strength, Ultimate, Minimum Guaranteed
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio, Calculated
  • Shear Modulus
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Niobium, Nb (Columbium, Cb)
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.