Available Properties |
---|
- Specific Gravity, JIS-K-6220; ASTM D-792
- Specific Gravity, JIS-K-6220; ASTM D 792, -40°C for 1,000 hrs
- Specific Gravity, JIS-K-6220; ASTM D 792, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Specific Gravity, JIS-K-6220; ASTM D 792, 80°C for 1,000 hrs
- Specific Gravity, JIS-K-6220; ASTM D 792, 85°C for 1,000 hrs with 85% RH
- Specific Gravity, JIS-K-6220; ASTM D 792, 125°C for 1,000 hrs
- Hardness, Shore C, SRIS0101S, 85°C for 1,000 hrs with 85% RH
- Hardness, Shore C, SRIS0101S, -40°C for 1,000 hrs
- Hardness, Shore C, SRIS0101S, 80°C for 1,000 hrs
- Hardness, Shore C, SRIS0101S, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Hardness, Shore C, SRIS0101S, 125°C for 1,000 hrs
- Hardness, Shore OO, ASTM D-2240
- Tensile Strength, Yield, JIS-K-6251(#2)/ASTM D-412
- Tensile Strength, Yield, JIS-K-6251(#2); ASTM D412, -40°C for 1,000 hrs
- Tensile Strength, Yield, JIS-K-6251(#2); ASTM D412, 85°C for 1,000 hrs with 85% RH
- Tensile Strength, Yield, JIS-K-6251(#2); ASTM D412, 80°C for 1,000 hrs
- Tensile Strength, Yield, JIS-K-6251(#2); ASTM D412, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Tensile Strength, Yield, JIS-K-6251(#2); ASTM D412, 125°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2); ASTM D412, 125°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2); ASTM D412, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Elongation at Yield, JIS-K-6251(#2)/ASTM D-412
- Elongation at Yield, JIS-K-6251(#2); ASTM D412, -40°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2); ASTM D412, 80°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2); ASTM D412, 85°C for 1,000 hrs with 85% RH
- Tear Strength, JIS-K-6252 (Angle)/ASTM D-624
- Tear Strength, JIS-K-6252(Angle); ASTM D624, -40°C for 1,000 hrs
- Tear Strength, JIS-K-6252(Angle)/ASTM D 624, 80°C for 1,000 hrs
- Tear Strength, JIS-K-6252(Angle); ASTM D 624, 85°C for 1,000 hrs with 85% RH
- Tear Strength, JIS-K-6252(Angle); ASTM D 624, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Tear Strength, JIS-K-6252 (Angle); ASTM D 624, 125°C for 1,000 hrs
- Volume Resistivity, JIS-K-6249; ASTM D257, -40°C for 1,000 hrs
- Volume Resistivity, JIS-K-6249/ASTM D257
- Volume Resistivity, JIS-K 6249; ASTM D257, 85°C for 1,000 hrs with 85% RH
- Volume Resistivity, JIS-K-6249; ASTM D149, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Volume Resistivity, JIS-K-6249; ASTM D 257, 80°C for 1,000 hrs
- Volume Resistivity, JIS-K-6249; ASTM D257, 125°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249; ASTM D149, -40°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249; ASTM D-149
- Dielectric Strength, JIS-K-6249; ASTM D 149, 80°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249; ASTM D 149, 125°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249; ASTM D 149, -40°C for 30 min and 125°C for 30 min. for 1,000 times
- Thermal Conductivity, JIS-R-2618; ASTM D2326
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flammability, UL94
|
| | |