Arnitel® ID 2045 is a highly flexible TPC (thermoplastic copolyester) that can be used in a broad range of applications from sports mouth guards to electronics. It is a flexible polymer with very good UV- and chemical-resistance compared to other flexible polymers such as TPU (thermoplastic urethane).
Arnitel® ID 2045 is an ECO label filament made with 50% bio-based feedstock which passes USP class IV, ISO 10993-10 Irritation / Intracutaneous reactivity as well as ISO 10993-5 Cytotoxicity tests. It combines easy and fast printing with high performance characteristics enabled by excellent inter-layer adhesion due to its slower crystallization behavior.
The mechanical data is tested on printed tensile bars, printed in two directions: 0°-90° and 45°-45°
The material passed the ISO irritation, ISO cytotoxicity and the USP VI tests.
Sustainability: Bio-based - 14C measurable
Special features: Contains renewable content
Processing technology: 3D printing
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic