MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Wacker Geniomer® 200 Silicone TPE Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Silicone, Thermoplastic

Material Notes: SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase. On account of its structure and the high siloxane content, the material is highly flexible and combines excellent transparency with good mechanical properties. SLM TPSE 200 contains neither plasticizers nor reinforcing fillers. It can be processed using standard thermoplastic processing techniques, and is particularly suitable for injection molding because of its low melt viscosity.

The high siloxane content prevents impairment of the elastomeric properties at low temperatures. SLM TPSE 200 can be coated with solvent-based paints, some of which may require the use of a suitable primer. Severe mechanical deformation of the elastomer may cause cracks in the coating due to the limited flexibility of the paint.

Suggested applications:

  • Production of industrial elastomeric components (including thin-walled components)
  • Processing aid for plastics extrusion
  • Hydrophobic, breathable textile coatings

Information provided by Wacker Silicones.

Vendors:
Available Properties
  • Density
  • Water Absorption at Saturation, By Thermogravimetry
  • Viscosity, Melt; Oscillating cone-plate
  • Viscosity, Melt; Oscillating cone-plate
  • Hardness, Shore A, DIN 53505
  • Tensile Strength at Break, DIN 53504 S2
  • Elongation at Break, DIN 53504 S2
  • 50% Modulus, DIN 53504 S2
  • 100% Modulus, DIN 53504 S2
  • Tear Strength, ASTM 624, Die B
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Compression Set, ISO 815, 40°C
  • Specific Heat Capacity, DSC
  • Specific Heat Capacity, DSC
  • Refractive Index
  • Transmission, Visible, Transparent; thickness not quantified
  • Processing Temperature, Metering Zone
  • Feed Temperature
  • Mold Temperature
  • Injection Pressure, Melt Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.