MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ascend Performance Materials Vydyne® 833F Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: Vydyne 833F is a PA66-based copolymer that features good melt strength (ideal for cast film and certain blown film processes), shear thinning behavior, high tensile strength, ductility, and slow crystallinity that matches crystallization temperatures/rates very close to that of ethylenes. The combination of properties exhibited by Vydyne 833F make it a good candidate for a number of applications such as numerous film uses, sheeting, and monofilament. The slow crystallization behavior coupled with the melting point ~ 215-220°C and great mechanical properties makes this material extremely useful for outside layers or internal layers of the multilayer film. This material further exhibits a very high elongation to break (> 500%) allowing for high draw ratios for thermoforming or when orienting the film.

Information provided by Ascend Performance Materials.

Vendors:
Available Properties
  • Bulk Density, ASTM D1895
  • Density, ISO 1183
  • Moisture Absorption, ASTM D6869
  • Viscosity Measurement, ISO 307, Relative Viscosity - Sulfuric Acid
  • Viscosity Measurement, ASTM D789, Relative Viscosity - Formic Acid
  • Puncture Resistance, ASTM F1306, Cast Film, Conditioned
  • Film Elongation at Break, MD, ASTM D882, Cast Film, Conditioned
  • Film Elongation at Break, MD, ASTM D882, Cast Film, Conditioned
  • Film Elongation at Break, TD, ASTM D882, Cast Film, Conditioned
  • Film Elongation at Break, TD, ASTM D882, Cast Film, Conditioned
  • Film Elongation at Yield, MD, ASTM D882, Cast Film, Conditioned
  • Film Elongation at Yield, TD, ASTM D882, Cast Film, Conditioned
  • Secant Modulus, MD, ASTM D882, Cast Film, Conditioned
  • Secant Modulus, MD, ASTM D882, Cast Film, Conditioned
  • Secant Modulus, TD, ASTM D882, Cast Film, Conditioned
  • Secant Modulus, TD, ASTM D882, Cast Film, Conditioned
  • Elmendorf Tear Strength MD, ASTM D1922, Cast Film, Conditioned
  • Elmendorf Tear Strength TD, ASTM D1922, Cast Film, Conditioned
  • Dart Drop Test, ASTM D1709A, Cast Film, Conditioned
  • Film Tensile Strength at Break, MD, ASTM D882, Cast Film, Conditioned
  • Film Tensile Strength at Break, TD, ASTM D882, Cast Film, Conditioned
  • Melting Point, ISO 11357-3
  • Shrinkage, MD, ASTM D1204, Cast Film, Conditioned
  • Shrinkage, TD, ASTM D1204, Cast Film, Conditioned
  • Processing Temperature, Blow Film Air Temperature
  • Processing Temperature, Cylinder - Extrusion
  • Die Temperature, Extrusion
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  • Moisture Content, Extrusion
  • European Food 1935/2004
  • FDA, 21CFR 177.1500
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Ascend Performance Materials (formerly Solutia)

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.