MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ExxonMobil 320 Mobil SHC PM Series
Categories: Fluid; Lubricant

Material Notes: Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide exceptional lubrication characteristics not attainable with conventional premium mineral oil-based fluids. The Mobil SHC PM Series oils are formulated to provide maximum protection of gears and bearings operating under the most severe conditions. They have very low pour points and a naturally high viscosity index (VI) which helps ensure good low temperature start-up while maintaining excellent viscosity characteristics at very high temperatures. The fluids are very shear stable and maintain viscosity control even when subjected to severe mechanical shear in heavily loaded bearings and gears. Their low traction coefficient and high viscosity index can help result in lower energy consumption and reduced component operating temperatures. Mobil SHC PM Series oils are formulated with synthesised hydrocarbon fluid (SHF) base oil technology and a proprietary additive system carefully balanced to attain high performance standards These fluids permit the use of higher steam pressures, temperatures and machine speeds common in high output paper machines and calendar rolls. Their outstanding hydrolytic stability and filterability assure excellent performance in the presence of water and the ability to retain effective filtration even at very fine filtration levels. They readily separate water and retain their colour characteristics for extended periods of operation under severe conditions.

Lubrication of severe industrial paper machine circulating systems; Application involving circulation systems operating over a wide temperature range such as calendar rolls; Systems that must be started and brought on line quickly; Circulation systems lubricating gears and bearings

Vendors:
Available Properties
  • Specific Gravity, ASTM D1298
  • Viscosity Measurement, ASTM D2270, Index
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Total Acid Number, ASTM D2619, Hydrolytic Stability (Acid Number Change), mgKOH/g
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.