MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Elantas Conap AD-1147 High Strength Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: AD-1147-C is a high-strength adhesive containing a stable solution of polymers in a solvent blend. It is developed specifically for bonding liquid urethanes to various substrates during the curing process. An extensive evaluation has demonstrated this system to be capable of bonding an exceptional variety of inorganic and organic materials together. AD-1147-C has a low solid content and requires heat to affect cure. Bonds to aluminum alloys, magnesium, iron, steel, glass, glass-fiber laminates, wood and leather have high strength and excellent resistance to hydrolysis and environmental extremes.

Features and Benefits: High strength / exceptional peel strength, Excellent resistance to hydrolysis and environmental extremes.

Vendors:
Available Properties
  • Specific Gravity, Conap AD-10147-C
  • Specific Gravity, Conap AD-1147
  • Solids Content, Conap AD-1147-C
  • Solids Content, Conap AD-1147
  • Viscosity, Conap AD-1147-C
  • Viscosity, Conap AD-1147
  • Shelf Life, Conap AD-1147. From date of manufacture unopened in the original containers.
  • Shelf Life, Conap AD-1147-C. From date of manufacture unopened in the original containers.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Elantas; Former Cytec product

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.