MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains its fibrous nature to 2480°C. The stabilized zirconia composition permits the advantages of fibrous insulations to be extended into temperature regions well above the melting temperatures of siliceous and alumina insulation materials.

Zirconia Felt Type ZYF-S.75G is ZYF-100 which has been physically filled with 0.75 grams silica per gram ZYF. This filled product retains some flexibility.

Features:

  • Low Thermal Conductivity
  • High Porosity
  • High Purity
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Custom Fillers and Coatings Available
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZIR-RIG
  • Easily Cut to Size
  • Available “Off the Shelf”

Application Information:

  • This heavy, silica loaded felt is used as a gasket material in molten carbonate fuel cells. When compressed between the sealing surfaces of the fuel cell container ZYF-S.75G forms a barrier that resists attack from the molten carbonate electrolyte.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors:
Available Properties
  • Bulk Density
  • Porosity, Bulk
  • Thickness
  • Compressive Yield Strength, At 10% compression
  • Shrinkage, 1 hour isothermal soak at 3000°F
  • Al2O3
  • HfO2
  • SiO2
  • ZrO2+Y2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.