MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ExxonMobil Thermrex Series V-32
Categories: Fluid; Quenchant

Material Notes: The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and thermal stability, demulsibility, and nonferrous compatibility. The use of such ingredients results in quench oils that provide uniform steel hardness, long batch life, resistance to sludge formation, and minimum deformation. Thermrex D-10, R-21, and V-32 are mineral-oil blends carefully selected to approximate 100 SUS at 100°F. They yield consistent Relative Cooling Indices (RCI) of 95 to 160. Thermrex F-43 is a fast quench oil augmenting selected base stocks with additive technology to provide an RCI of 195. In addition, Thermrex R-21, V-32, F-43 are "gapped" to yield controlled distillation ranges from specific base stocks.

The Thermrex Series oils are excellent media for rapidly cooling alloy steels to achieve optimum strength and toughness. The selection of the particular grade of quench oil depends on the cooling rate desired to prevent cracking and distortion. Thermrex Series oils D-10, R-21, V-32, and F-43 are most effective with agitation at batch temperatures of less than 150°F.

Vendors:
Available Properties
  • Specific Gravity
  • Kinematic Viscosity at 40°C (104°F)
  • Pour Point
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.