MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Versalis Revive® EPS 3000 Expanded Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Revive® EPS 3000 has been developed for sustainable packaging: it contains the 20% of secondary raw material and a lower pentane content for the lower emissions. Versalis Revive® EPS 3000 has the same performances of the standard EPS for packaging. The narrow bead size distribution lead to good filling of the molds and allow to obtain a very smooth surface. The color of the raw material may change depending on the secondary raw material, once expanded the color will be pearl-white.

Applications: Versalis Revive® EPS 3000 is recommended for shape molding of: protective white goods packaging, protective industrial packaging, Versalis Revive® EPS 3000 is not suitable for food contact applications.

Information provided by Versalis.

Vendors:
Available Properties
  • Bulk Density
  • Density, Discontinuous pre-expander.
  • Density, continuous pre-expander after one expansion
  • Density, Normal Density Range
  • Particle Size
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polimeri Europa (Former Polimeri Europa (EniChem)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.